Environment-friendly ‘ITmk3’ process plant for production of iron nuggets by Kobe Steel
Kobe Steel Limited has announced that the world's first commercial plant using the ITmk3® Process successfully began production of iron nuggets in the United States on January 12th 2010. The next generation ITmk3 Process was developed by Kobe Steel.
Kobe Steel and Steel Dynamics Inc constructed the plant at Hoyt Lakes in Minnesota. Production of iron nuggets, which are used in steelmaking, will gradually increase in accordance with operating conditions and is anticipated to reach the facility's annual design capacity of 50,000 tonnes in mid 2010.
ITmk3 is an innovative next generation iron making process totally different in concept from the traditional blast furnace method. Since the discovery of the phenomenon in 1994, the process has undergone many stages of development resulting in the start of production of a commercial plant.
* The ITmk3 Process is noted for the following characteristics:
1. High grade iron nuggets can be produced in an extremely short time of about 10 minutes
2. The ITmk3 Process can use lower cost iron ore fines and steaming coal, which are difficult to use in blast furnace iron making
3. In comparison to pig iron produced in a blast furnace, the production of iron nuggets using the ITmk3 Process emits about 20% less carbon dioxide due to its good energy efficiency
With the start up of the commercial ITmk3 plant, Kobe Steel is moving quickly to popularize the ITmk3 Process in world markets. As a pioneer of this technology, Kobe Steel is working on iron nugget projects in North America, Vietnam, India, Russia, Australia and other countries, a cumulative production capacity of several million tonnes of iron nuggets.
Over the medium to long term future, steel demand is anticipated to continue increasing. Accordingly, electric arc furnace steelmakers are faced with a growing need for cold iron units, namely clean iron units such as blast-furnace pig iron and direct reduced iron. Kobe Steel believes the ITmk3 Process is one of the most effective ways to meet this new demand.
The ITmk3 Process, with its lower carbon-dioxide emissions and capital investment, is highly suitable for growing environmentally friendly steel industries in developing countries. Moreover the ITmk3 Process can use cheaper low grade iron ore and coal, which are difficult to use in blast furnace iron making, to keep raw material costs down for steel and mining companies. Along with these advantages, the real value of the ITmk3 Process is that it produces high-grade iron nuggets with better meltability than blast-furnace pig iron when used in the steelmaking stage.
For mining companies, the ITmk3 Process enables them to produce iron nuggets to add value to their natural resources. As a result, mining companies can expand their markets to include electric arc furnace steelmakers, in addition to their traditional customers, blast furnace steelmakers.
Grappling with environmental issues, the world steel industry faces a tight raw material market and higher costs due to the sharp increase in steel production. Under these conditions, the ITmk3 Process is an attractive alternative. Kobe Steel, with subsidiary Midrex Technologies Inc is the world's leader in direct reduction processes. Its MIDREX® Direct Reduction Process is used to produce nearly 60% of the world's direct reduced iron. As a member of the world steel industry, Kobe Steel has now commercialized ITmk3, a revolutionary iron making process that, in step with the present age, contributes to society.
* The ITmk3 Process
1. Pulverized iron ore and pulverized coal are agglomerated into ball-shaped pellets
2. The pellets are fed into a rotary hearth furnace. Reduction, melting and slag separation occur in about 10 minutes
3. The resulting product is high-grade iron nuggets
*Advantages of the ITmk3 Process
1. In comparison to pig iron produced in a blast furnace, the production of iron nuggets using the ITmk3 Process emits about 20% less carbon dioxide due to its good energy efficiency
2. Raw material pretreatment facilities (coke ovens, sintering plants and pellet plants) are unnecessary
3. ITmk3 is highly suitable for mining sites and can be profitable for even small mines
4. Operation is easy and production adjustments are also easy.
* Features of the Iron Nuggets
1. Iron nuggets are slag-free, high-purity iron units of the same quality as pig iron. They have a metallic iron content of 96% to 97%
2. Iron nuggets improve the productivity and energy efficiency of electric arc furnaces. With better meltability than blast furnace pig iron, iron nuggets can be continuously fed into EAFs
3. Iron nuggets are easy to transport and handle. High in density, they do not re oxidize or generate fines.
(Sourced from Kobe Steel)
Ref.: http://steelguru.com/article/details/Nzk%3D/Commercial_operation_of_ITmk3_plant_in_USA_-_Kobe_Steel.html
Tuesday, March 4, 2008
Steel making:


Steel making:
After iron is obtained either from blast furnace in liquid / melt form (pig iron) or from DRI (sponge iron) process; it is sent for steel production. The iron that emerges from the blast furnace contains 4 - 4.5 % carbon by wt., and other impurities which makes the metal too brittle for most engineering applications. The Basic Oxygen Steelmaking (BOS) process takes this liquid iron plus recycled scrap steel, and reduces the carbon content to between 0 and 1.5% by blowing oxygen through the metal.
Steel is generally made by the Bessemer, Siemens Open Hearth, basic oxygen furnace, electric arc, electric high-frequency and crucible processes.
In Bessemer (BOS) process molten pig iron is refined by blowing air through it in an egg-shaped vessel, known as a converter. In the Siemens process, the necessary heat for melting and working the charge is supplied by oil or gas. Both the gas and air are preheated by regenerators. The regenerators are chambers filled with checker brickwork, brick and space alternating.
The high nitrogen content of
The least costly method of making steel uses scrap metal as its base. Steel scrap from many sources—such as old bridges, refrigerators, and automobiles—and other additives are placed in an electric arc furnace, where the intense heat produced by carbon electrodes and chemical reactions melts the scrap, converting it into molten steel.
Most of these steel plants have finishing mills on site that convert iron and steel into both finished and intermediate products. Some of the goods produced in finishing mills are steel wire, pipe, bars, rods, and sheets. While wire, steel reinforcing bars, and pipes are considered finished products, rolled steel is intermediates, meaning it is normally shipped to companies, such as automotive plants, that stamp, shape, and machine the rolled steel into car parts. In these finishing mills, products also may be coated with chemicals, paints, or other metals that give the steel desired characteristics for various industries and consumers.
Steel manufacturing is an intensely competitive global industry. By continually improving its manufacturing processes and consolidating businesses many of the steel companies increased productivity sufficiently to remain competitive in the global market for steel.
Monday, March 3, 2008
Direct reduction of iron (DRI) – ‘Sponge iron’

Direct reduction of iron (DRI) – ‘Sponge iron’, another method of producing iron:
All steelmaking processes require the input of iron bearing materials as process feedstock. For making steel in a basic oxygen furnace, the iron bearing feed materials are usually blast furnace hot metal and steel scrap. A broadly used iron source is also a product known as Direct Reduced Iron ("DRI") which is produced by the solid state reduction of iron ore to highly metallized iron without the formation of liquid iron. This solid state reduction of iron ore is also called ‘sponge iron’.
Sponge iron is the product created when iron ore is reduced to metallic iron, in the presence of coal, at temperatures below the melting point of iron. The external shape of the ore is retained with 30% reduction in weight due to oxide reduction resulting in change in true density from 4.4 gm/cc to 7.8 gm/cc in this product. This paves the way for 54% reduction in volume which is manifested in pore formation through out the interior of reduced product and hence the name “Sponge Iron”. This spongy mass sometimes called a bloom. This makes for an energy-efficient feedstock for specialty steel manufacturers which used to rely upon scrap metal. The advantage of this technique is that iron can be obtained at a lower furnace temperature (only about 1,100°C or so). Only small quantities of sponge iron can be made at a time as compare to blast furnace process, is the major disadvantage.
In this method, the iron ore along with coal is charged to the top portion of the reduction zone of a rotary kiln or furnace, wherein the bed of particles which descend by gravity is reduced by a hot reducing gas largely composed by carbon monoxide (CO) and hydrogen (H2). Finally, the product sponge iron is discharged from the bottom portion of the discharge zone of the furnace and conveyed (after cooling), for example, to be melted in an electric arc furnace or to be briquetted in a briquetting machine coupled to the reduction reactor. The evolution of sponge iron as a metallic feed in electric steel making has been mainly due to reduced availability of high quality scrap and its increasing cost.
Quality of sponge iron for steel making: There are several parameters to be monitored for improving the quality of sponge iron for steel making operation, such as – (a) Size, (b) Density, (c) Unit weight, (d) Crushing strength, (e) Weather resistance, (f) Carbon contents, (g) Metallization.
(a) Size - The size of sponge iron is very important especially with regard to continuous feeding. A very fine sized material (1 mm to 2 mm) would be quickly oxidized during falling to the slag or may be lost in fume extraction system. Extremely large size (exceeding 30 mm) poses problem during continuous feeding. The size fraction less than 2 mm needs to be limited for continuous feeding.
(b) Density - Sponge iron after falling should have the ability to penetrate into the slag layer and reside at the slag/metal interface for effective heat transfer and chemical reaction. Sponge iron with lower density tend to float on the slag while, high density material readily penetrates into the metal. Hence, it is desirable to have the density of sponge iron in the range 4 - 6 gm/cc.
(c) Unit weight – The transition time of the sponge iron pellets through the slag is dependant on the momentum. If the pellet stays in the slag layer for too long a time, the phenomenon of slag boiling occurs. Slag fluidity is highly important. However, a heavier sponge iron pellet does not require close control in slag fluidity.
(d) Crushing strength - Sponge iron should possess good crushing strength to prevent generation of large amounts of fines.
(e) Weather resistance - Sponge iron is prone to oxidation and heat builds up in contact with atmosphere. The storage of Sponge Iron for long periods of time affects its metallization, partially due to surface re-oxidation caused by the porous structure of sponge iron pellets or lumps.
(f) Carbon contents - During continuous feeding, an active carbon — oxygen boil is necessary to shield the arcs. It has been observed that to achieve the aforesaid, sponge iron should possess a minimum of 0.60% carbon.
(g) Metallization - High metallization helps in lower power consumption but severely reduces the bath activity and results in flat bath conditions. For low metallization levels, increased carburization is required to compensate for the extra oxygen in sponge iron.